SW Activated Ceramic Ball
|
[ Products Description ]
SW Activated ceramic ball is a new support material for catalyst. It is processed by adding a small amount of transition metal oxide into the inert ceramic ball. It preserve the property of high-temperature resistance and strength of the inert ceramic ball, in addition. It has adequate catalytic activity when used in the process of olefin hydrogenation. If been set on the top of catalyst bed in the reactor, the activated ceramic ball can make the olefin in the secondary processing fraction pre-hydrogenated and, keep the catalyst from cokings. Similarly, if been set on the bottom, it can remove the thio-alcohol caused in the reaction process. On the whole, using the SW activated ceramic ball can not only save the space in reactor, but also protect the catalyst from poisoning or sintering and, consequently prolong the service life of catalyst.
[ Technical Specification ]
Item/Type |
SW-1 |
SW-2 |
SW-3 |
Appearance |
Tan |
Light yellow |
Light gray |
Bulk density g/ml |
1.1-1.3 |
1.1-1.3 |
1.1-1.3 |
Porosity |
0.1-0.20 |
Thermal Resistance, °C |
500 |
500 |
500 |
Crushing Strength |
130-3500 |
Abrasion |
<2% |
Al2O3 Content |
≥40 |
≥40 |
≥40 |
Active component |
NiO.MoO3 |
NiO.WO3 |
CoO.MoO3 |
|
Note: The data of bulk density is given for reference only, not as the acceptance criterion.
[ Catalytic Property ]
Item/Type |
SW-1 |
SW-2 |
SW-3 |
Reaction temperature, °C |
275 |
300 |
300 |
320 |
350 |
300 |
320 |
350 |
Hydrogen pressure, MPa |
3.0 |
3.0 |
3.0 |
3.0 |
3.0 |
3.0 |
3.0 |
3.0 |
Liquid velocity, h-1 |
10 |
10 |
4.2 |
4.2 |
4.2 |
4.2 |
4.2 |
4.2 |
Ratio of hydrogen/oil |
600 |
600 |
450 |
450 |
450 |
450 |
450 |
450 |
Sulfur content, Wt% |
2.5 |
2.5 |
2.5 |
2.5 |
2.5 |
2.5 |
2.5 |
2.5 |
Olefin content, Wt% |
27.5 |
27.5 |
27.5 |
27.5 |
27.5 |
27.5 |
27.5 |
27.5 |
Rate of desulfation, % |
76 |
95 |
40 |
60 |
77 |
36 |
54 |
63 |
Olefin saturation, % |
58 |
95 |
10 |
33 |
45 |
7 |
19 |
42 |
|
|